Exaton 25.22.2.LMn is a chromium-nickel-molybdenum strip electrode used for electro-slag welding (ESW) or submerged arc welding (SAW) to deposit a second layer corrosion resistant alloy of 25%Cr/22%Ni/2%Mo composition on carbon- and low alloyed steels. It can also be used as buffer layer before depositing second layers.

Категория:
Загрузка...

Описание

Exaton 25.22.2.LMn is a chromium-nickel-molybdenum strip electrode used for electro-slag welding (ESW) or submerged arc welding (SAW) to deposit a second layer corrosion resistant alloy of 25%Cr/22%Ni/2%Mo composition on carbon- and low alloyed steels. It can also be used as buffer layer before depositing second layers.



Классификации

Классификации EN ISO 14343-A : B 25 22 2 N L
SFA/AWS A5.9 : EQ»310LMo»

Хим. состав наплавленного металла

Хим. состав проволоки
C Cr Mn Mo N Ni P S Si
&lt.=0.020 % 25.0 % 4.5 % 2.1 % 0.13 % 22.0 % &lt.=0.015 % &lt.=0.015 % &lt.=0.2 %

Отзывы

Отзывов пока нет.

Будьте первым, кто оставил отзыв на “Exaton 25.22.2.LMn”

Ваш адрес email не будет опубликован. Обязательные поля помечены *

КАТАЛОГ